Flow Level Pressure
Quality Monitoring of Pipelines
Nov 24 2015
Buried gas and water lines made of steel are endangered by external corrosion. Even after the introduction of cathodic corrosion protection in the early 1960s, pipelines still have to be protected from corrosion by a pore-free coating. Only in this way can gas and water suppliers ensure long-term protection of their investment costs in their pipeline network.
To ensure that the factory coating and the coating applied at the work site are free of pores, these are supplied with high voltage between the steel pipe and a test electrode. If a spark-over occurs here, this indicates a defect in the coating. This coating must be touched up and then undergo another test.
UNION Instruments (Germany) offers the mobile UIP insulation tester for reliable testing of pipe coatings for defects. With adjustable test voltages of 5 kV to 30 kV and a comprehensive assortment of corresponding test electrodes, the coated pipes and system components can be quickly and reliably tested. The battery-powered device operates for many hours without recharging. Thus, even long pipelines or large areas can be efficiently checked. Typical applications of the device are pipeline construction and liquid gas tanks.
Digital Edition
PIN 25.1 Feb/March
March 2024
In This Edition Safety - The technology behind the ION Science Tiger XT - Safety with ammonia and LOHCs as hydrogen carriers Analytical Instrumentation - Discussion on new tribology te...
View all digital editions
Events
Apr 03 2024 Tashkent, Uzbekistan
Salon Analyse Industrielle & Instrumentation
Apr 03 2024 Paris, France
Apr 03 2024 Atyrau, Kazakhstan
Apr 09 2024 Munich, Germany
Apr 10 2024 Helsinki, Finland